Defects of coating
Finished coating is too soft
If you encounter this problem after the powder coatings have cured, perform a step-by-step check of the technology parts mentioned below.
1 ze 4
Application equipment
- improper application method
Application equipment setup
- electrostatic deposition voltage set too high
- poorly adjusted manipulator dead center – on the edge
- improper setting of the voltampere characteristic
- air pressure set too high (the powder is blown off towards the edges)
Paint (powder coating)
- defective powder coating batch
- wet powder coating
- the powder is too fine:
- the recycled material content is too high
- too fine from production
Part and its hanging
- insufficiently grounded part
Curing oven
- the temperature rise during the powder coating curing is too slow